Physical Properties | Metric | English | Comments |
---|---|---|---|
Bulk Density | 2.05 - 2.15 g/cc | 0.0741 - 0.0777 lb/in³ | After drying at 110°C |
Gouda Vuurvast CURON 130 HRCC RAPID Dense Refractory Castable Description: An extra coarse, low iron castable for use to 1300°C under normal operation conditions, also usable under reducing circumstances. Curon 130 HRCC RAPID has good thermal shock resistan.. |