Physical Properties Metric English Comments
Bulk Density 1.78 g/cc
0.0643 lb/in³
Du-Co Ceramics S-470 Aluminum Silicate
Du-Co Ceramics Company manufactures a variety of crushable ceramic materials for use worldwide in cartridge heaters, thermocouples, and mineral insulated cable. The crushable ceramic products are cu..
Bulk Density 1.78 g/cc
0.0643 lb/in³
Chosun Refractories MS-2 Blast Furnace Tap-Hole Refractory
Information provided by Chosun Refractories via Korea Institute of Ceramic Engineering and Technology (KICET).