Physical Properties | Metric | English | Comments |
---|---|---|---|
Bulk Density | 1.59 g/cc | 0.0573 lb/in³ | Tapped; ASTM D 3101-78 |
Potters Industries Spheriglass® 3000 Solid Glass Spheres Description: Spheriglass® fine solid glass spheres are used as an additive for thermoplastic and thermosetting resin systems. Glass spheres give products many benefits such as:Low Uniform Shrinkage.. |
|||
Bulk Density | 1.59 g/cc | 0.0573 lb/in³ | Loose |
Excalibar ExBar™ W 325 Barite BaSO4 Powder ExBar™ W high-purity white barytes are manufactured using only the highest quality white, natural barium sulfate ore. Strict quality control results in consistent products that are used in paints, .. |