Polymer Property : Bulk Density = 1.56 g/cc
Polymer Property :
Bulk Density =
1.56 g/cc
Product List
Physical Properties
Tips:
30 items are displayed at most. For the rest of the results, please contact customer service.
Physical Properties
Metric
English
Comments
Bulk Density
1.56
g/cc
0.0562
lb/in³
Powder
Aremco Ceramacast™ 900 High Temperature Potting & Casting Material Zirconia Silicate
High Density, high strength molding compound.