Polymer Property : Bulk Density = 1.55 g/cc Product List

Physical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Physical Properties Metric English Comments
Bulk Density 1.55 g/cc
0.0560 lb/in³
Tapped
Nyco HARRP™ 20 X 40 Wollastonite
HARRP™ 20X40 is suggested for concrete and concrete roof tile reinforcement.Wollastonite is a naturally occurring white mineral with an acicular (needle-shaped) particle structure. This distinctive..
Bulk Density 1.55 - 1.65 g/cc
0.0560 - 0.0596 lb/in³
3M 7000 Series Copper Roofing Granule (Wausau)
3M Copper Roofing Granules are ceramic-coated minerals used as surfacing material in asphalt roofing products. These granules are colored with durable pigments, bonded in a ceramic matrix and treate..