Polymer Property : Bulk Density = 1.35 g/cc Product List

Physical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Physical Properties Metric English Comments
Bulk Density 1.35 g/cc
0.0488 lb/in³
Packed
Omya OMYACARB® 6 - PT Calcium Carbonate
A dry ground calcium carbonate with intermediate and closely sized particle distribution.Applications: An ideal extender for plastics, rubber, coating, and caulks. Designed for use in unsaturated po..
Bulk Density 1.35 - 1.45 g/cc
0.0488 - 0.0524 lb/in³
After drying at 110°C
Gouda Vuurvast GOLITE 135 Refractory Insulating Castable
Description: Golite 135 can be used in direct contact with fire and combines a good strength with a high insulation value.Remarks: These values apply to cast products. Also available in gunning vari..
Bulk Density 1.35 g/cc
0.0488 lb/in³
Sharadaa Ceramics 32 Insulation Bricks-ASTM
Services Offered: Retrofitting of Furnace, Installation of Castables/Bricks/Ceramic Fiber Modules, Castable Laying by Vibrocasting/Guiniting, Turnkey Installation Boiler/Chimney/Heater/Reformer/Rota..