Physical Properties | Metric | English | Comments |
---|---|---|---|
Bulk Density | 1.31 g/cc | 0.0473 lb/in³ | Tapped |
Nyco NYAD® M200 Wollastonite Wollastonite is a naturally occurring white mineral with an acicular (needle-shaped) particle structure. This distinctive particle morphology makes wollastonite an ideal performance mineral for a br.. |
|||
Bulk Density | 1.31 g/cc | 0.0473 lb/in³ | Tapped |
Nyco NYAD® MD200 Wollastonite Wollastonite is a naturally occurring white mineral with an acicular (needle-shaped) particle structure. This distinctive particle morphology makes wollastonite an ideal performance mineral for a br.. |
|||
Bulk Density | 1.31 g/cc | 0.0475 lb/in³ | Untapped; ASTM D 3101-78 |
Potters Industries Spheriglass® 3000E Solid Glass Spheres Description: Spheriglass® fine solid glass spheres are used as an additive for thermoplastic and thermosetting resin systems. Glass spheres give products many benefits such as:Low Uniform Shrinkage.. |