Physical Properties | Metric | English | Comments |
---|---|---|---|
Bulk Density | 1.06 g/cc | 0.0382 lb/in³ | Defined by casting method, +/- 50kg (110 lbs) |
Skamol Group SKAMOCAST 14-105 Insulating Castable SKAMOL insulating castables have the following characteristics: Max. service temperature: Up to 1100°C (2102°F)Back-up insulation or hot-face usesFor casting and gunningProducts are based on f.. |
|||
Bulk Density | 1.06 g/cc | 0.0383 lb/in³ | |
DuPont™ Nomex® 410 Paper, 20 mil Nominal Thickness Nomex® Type 410 is a calendared insulation paper which offers high inherent dielectric strength, mechanical toughness, flexibility, and resilience. It is the original form of Nomex® paper and is .. |
|||
Bulk Density | 1.06 g/cc | 0.0382 lb/in³ | Tapped |
CIMBAR EliteTalc® 21 Cosmetic Talc Cimbar performance Minerals MV, LLC Talc U.S.P. Cosmetic talcs are designed specifically for cosmetic formulations. Talc is commonly used in cosmetics for its ability to bind to oils, create a mois.. |