Physical Properties | Metric | English | Comments |
---|---|---|---|
Bulk Density | 1.01 g/cc | 0.0365 lb/in³ | Loose |
Excalibar ExCal® CW 100 Calcium Carbonate CaCO3 Powder ExCal® CW calcium carbonate products are processed from a high-purity ore, to exacting specifications at the Houston, Texas plant. These grades are processed for use in plastics, rubber, coatings,.. |