Physical Properties Metric English Comments
Bulk Density 0.975 g/cc
0.0352 lb/in³
Powder; ASTM D1895
Sumitomo Bakelite North America FM 4004F Fiberglass and Mineral Reinforced Phenolic Novolac
FM 4004F is a fiberglass and mineral reinforced phenolic novolac compound with improved strength properties over FM 4004. This compound exhibits excellent dimensional stability and good strength at..