Physical Properties | Metric | English | Comments |
---|---|---|---|
Bulk Density | 0.858 g/cc | 0.0310 lb/in³ | Poured; ASTM D1895 |
Eastman CM01 PET
(discontinued **) Voridian Polymer CM01 is clear polymer that is available in North America. This product is useful for production of beverage, food, and edible oil containers.Applications/UsesCarbonated soft drink c.. |