Physical Properties | Metric | English | Comments |
---|---|---|---|
Bulk Density | 0.608 - 0.640 g/cc | 0.0220 - 0.0231 lb/in³ | Before expansion |
NOVA Chemicals Dylite® F271T Specialty Expandable Polystyrene Features: Highly consistent bead size; high gloss characteristics; low energy consumption; fast cyclingApplications: Drinking cups -hot and cold, noodle bowls, take-out and ice cream containers, and.. |