Physical Properties | Metric | English | Comments |
---|---|---|---|
Bulk Density | 0.455 g/cc | 0.0164 lb/in³ | Pour Density; ASTM D 1513 |
Orion Engineered Carbons CORAX® N 326 ASTM Carbon Black Standard grade of furnace black in accordance with the requirements of ASTM D 1765Hard Black - tread grade, reinforcing carbon blackInformation provided by Orion Engineered Carbons. |