Physical Properties | Metric | English | Comments |
---|---|---|---|
Bulk Density | >= 6.00 g/cc | >= 0.217 lb/in³ | |
China-Yixing Longly Refractories Zirconia Ceramics LONGLY provides a multitude of zirconia products including balls, plates, tubes, rods and etc. by adopting magnesia, calcia or yttria stabilized zirconia powder as raw material through dry pressing,.. |
|||
Bulk Density | 6.01 g/cc | 0.217 lb/in³ | |
Astro Met AmZirOx 86 Zirconia - Zirconium Oxide General Description:AmZirOx 86 zirconia (Astro Met Zirconium Oxide) is a yttria stabilized zirconia ceramic material which features high strength and toughness making it a candidate material for use.. |