Polymer Property : Bulk Density = 0.142 lb/in³ Product List

Physical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Physical Properties Metric English Comments
Bulk Density 3.93 g/cc
0.142 lb/in³
Astro Met AmAlOx 68 Alumina - Aluminum Oxide
General Description:AmAlOx 68 alumina (Astro Met Aluminum Oxide) is a high purity 99.8% aluminum oxide (alumina) ceramic which has been developed and optimized for maximum wear resistance and corros..