Polymer Property : Bulk Density = 0.140 g/cc Product List

Physical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Physical Properties Metric English Comments
Bulk Density 0.140 g/cc
0.00506 lb/in³
Potters Industries Sphericel® 25P45 Hollow Engineered Glass Microspheres
Sphericel® hollow glass microspheres are alternatives to conventional fillers and additives such as silicas, calcium carbonates, talc, clay, etc. A variety of particle sizes, densities and strength..
Bulk Density 0.140 g/cc
0.00506 lb/in³
SPHERE ONE EXTENDOSPHERESâ„¢ XOL-200 Hollow Spheres
EXTENDOSPHERESâ„¢ XOL-200 are white aluminosilicate multicellular hollow spheres. The density of this product averages 0.25 g/cc. In plastic and coating applications, EXTENDOSPHERESâ„¢ XOL-200..
Bulk Density 0.140 - 0.160 g/cc
0.00506 - 0.00578 lb/in³
Tamped Bulk Density
Unipetrol A+ High-Conductive Carbon Black Chezacarb
Carbon black Chezacarb is manufactured by gasification of heavy petroleum residues by partial oxidation in Shell reactors. It is produced in the form of pellets of size 0,5 - 2,5 mm. Product is not ..
Bulk Density 0.140 g/cc
0.00506 lb/in³
Scott
TIMCAL TIMREX® F25 Primary Synthetic P/M Special-Graphite
TIMREX Primary Synthetic Graphite is produced in a unique highly controlled graphitization process which assures narrow specifications and unequalled consistent quality due to: monitoring of all pro..