Physical Properties | Metric | English | Comments |
---|---|---|---|
Bulk Density | 3.40 g/cc | 0.123 lb/in³ | |
Minelco MagnaDense 2 Fine Aggregate MagnaDense is a high grade natural aggregate, manufactured from the iron oxide Magnetite. With its high density MagnaDense is used as loose ballast or as aggregate to produce high quality, high dens.. |
|||
Bulk Density | 3.40 g/cc | 0.123 lb/in³ | |
Minelco MagnaDense 4 Fine Aggregate MagnaDense is a high grade natural aggregate, manufactured from the iron oxide Magnetite. With its high density MagnaDense is used as loose ballast or as aggregate to produce high quality, high dens.. |
|||
Bulk Density | 3.40 g/cc | 0.123 lb/in³ | |
China Tungsten YG13C Tungsten Carbide Information provided by China Tungsten |
|||
Bulk Density | 3.40 g/cc | 0.123 lb/in³ | |
China Tungsten YG4C Tungsten Carbide Information provided by China Tungsten |
|||
Bulk Density | 3.40 g/cc | 0.123 lb/in³ | |
China Tungsten YG6 Tungsten Carbide Information provided by China Tungsten |
|||
Bulk Density | 3.40 g/cc | 0.123 lb/in³ | Scott |
China Tungsten YG6 Tungsten Carbide Powder Information provided by China Tungsten |
|||
Bulk Density | 3.40 g/cc | 0.123 lb/in³ | |
China Tungsten YG6C Tungsten Carbide Information provided by China Tungsten |
|||
Bulk Density | 3.40 g/cc | 0.123 lb/in³ | Scott |
China Tungsten YG6C Tungsten Carbide Powder Information provided by China Tungsten |
|||
Bulk Density | 3.40 g/cc | 0.123 lb/in³ | |
China Tungsten YG8 Tungsten Carbide Information provided by China Tungsten |
|||
Bulk Density | 3.40 g/cc | 0.123 lb/in³ | |
China Tungsten YG8C Tungsten Carbide Information provided by China Tungsten |
|||
Bulk Density | 3.40 g/cc | 0.123 lb/in³ | Scott |
China Tungsten YG6X Tungsten Carbide Powder Information provided by China Tungsten |