Physical Properties | Metric | English | Comments |
---|---|---|---|
Bulk Density | >= 0.118 g/cc | >= 0.00426 lb/in³ | |
Unipetrol A+ High-Conductive Carbon Black Chezacarb Carbon black Chezacarb is manufactured by gasification of heavy petroleum residues by partial oxidation in Shell reactors. It is produced in the form of pellets of size 0,5 - 2,5 mm. Product is not .. |
|||
Bulk Density | 0.118 g/cc | 0.00425 lb/in³ | Loose |
BYK Cloisite® 20A Nanoclay Cloisite® 20A is an additive for plastics to improve various plastic physical properties, such as reinforcement, HDT, CLTE and barrier.Information provided by Southern Clay ProductsSouthern Clay Pr.. |