Physical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Physical Properties Metric English Comments
Bulk Density 2.90 - 3.00 g/cc
0.105 - 0.108 lb/in³
After drying at 110°C
Gouda Vuurvast CURAS 85 P Moldable Refractory Material
Description: This phosphate bonded material based on corundum and bauxite has already at low temperature a reasonable strength and has a very good resistance against slag attack or liquid aluminum. ..
Bulk Density 2.90 - 3.00 g/cc
0.105 - 0.108 lb/in³
After drying at 110°C
Gouda Vuurvast CURAS 90 PF REPAIR Moldable Refractory Material
Description: Curas 90 PF Repair ramming mix is especially developed for repairing purposes of Curas 90 PF linings. The product is supplied in two components: a dry powder and a liquid. Detailed inst..
Bulk Density 2.90 - 3.00 g/cc
0.105 - 0.108 lb/in³
After drying at 110°C
Gouda Vuurvast CURAS PBK D Moldable Refractory Material
Description: This material is supplied as a dry powder, it has to be mixed with potable water to the necessary consistency. This moldable contains a phosphate binding agent and has a low silica cont..
Bulk Density 2.90 - 3.00 g/cc
0.105 - 0.108 lb/in³
After drying at 110°C
Gouda Vuurvast CURAS PBK DGM Moldable Refractory Material
Description: This material is supplied as a dry gunning powder. This moldable contains a phosphate binding agent and has a low silica content. For a large variety of applications this results in goo..
Bulk Density 2.90 - 3.00 g/cc
0.105 - 0.108 lb/in³
After drying at 110°C
Gouda Vuurvast VIBRON 150 GZ (R) Dense Vibrating Refractory Castable
Description: Vibron 150 GZ (R) is a low cement castable based on sintered South-American bauxite. The addition of zircon oxide in this product makes it suitable for areas under heavy chemical attack..
Bulk Density 2.90 - 3.00 g/cc
0.105 - 0.108 lb/in³
After drying at 110°C
Gouda Vuurvast CURAS PBK Moldable Refractory Material
Description: This moldable contains a phosphate binding agent and has a low silica content. For a large variety of applications this results in a good slag resistance and high strength properties at..