Physical Properties | Metric | English | Comments |
---|---|---|---|
Bulk Density | 2.75 - 2.81 g/cc | 0.0994 - 0.102 lb/in³ | |
Chosun Refractories CUN-718 Nozzle Brick Information provided by Chosun Refractories via Korea Institute of Ceramic Engineering and Technology (KICET). |