Physical Properties | Metric | English | Comments |
---|---|---|---|
Bulk Density | 2.72 - 3.52 g/cc | 0.0983 - 0.127 lb/in³ | |
Reade Advanced Materials Zirconium Oxide, Hafnia Stabilized (ZrO2 + HfO2) Description: A fused high density monoclinic grain. Used in fluid beds as loose insulation, setting grain and as a source of zirconium.Forms Available: Available in both USS mesh and F sizesInforma.. |