Physical Properties | Metric | English | Comments |
---|---|---|---|
Bulk Density | 2.26 g/cc | 0.0816 lb/in³ | |
Chosun Refractories CRS-A60 Blast Furnace Tap-Hole Refractory Information provided by Chosun Refractories via Korea Institute of Ceramic Engineering and Technology (KICET). |
|||
Bulk Density | 2.26 g/cc | 0.0816 lb/in³ | |
Chosun Refractories MRC-7 Blast Furnace Tap-Hole Refractory Information provided by Chosun Refractories via Korea Institute of Ceramic Engineering and Technology (KICET). |