Physical Properties | Metric | English | Comments |
---|---|---|---|
Bulk Density | 2.21 g/cc | 0.0799 lb/in³ | |
Nyco HARRP™ 40 Wollastonite HARRP™ 40 is suggested for concrete, roof tile, grout/stucco, etc. reinforcement.Wollastonite is a naturally occurring white mineral with an acicular (needle-shaped) particle structure. This distin.. |