Physical Properties | Metric | English | Comments |
---|---|---|---|
Bulk Density | 1.97 g/cc | 0.0712 lb/in³ | Dipping, 7% H2O |
BNZ Materials Blakbond Mortar Blakbond is a highly refractory mortar which possesses high water retention properties. It is especially designed for laying insulating fire brick and is also used for super duty and high alumina de.. |