Physical Properties | Metric | English | Comments |
---|---|---|---|
Bulk Density | 0.0650 g/cc | 0.00235 lb/in³ | Scott |
TIMCAL TIMREX® MX15 Primary Synthetic Graphite TIMREX Primary Synthetic Graphite is produced in a unique highly controlled graphitization process which assures narrow specifications and unequalled consistent quality due to: monitoring of all pro.. |