Physical Properties Metric English Comments
Bulk Density 0.0641 g/cc
0.00232 lb/in³
Inhance Fluoro-Seal INHANCE® PEF High Density Fibrillated Polyethylene
Product Description: INHANCE PEF fiber is a high density fibrillated (highly branched) polyethylene fiber that has been surface activated by a proprietary reactive gas process. Surface activation m..