Physical Properties | Metric | English | Comments |
---|---|---|---|
Bulk Density | 1.38 g/cc | 0.0499 lb/in³ | Tapped |
Nyco M200 WOLLASTOCOAT® Wollastonite Wollastonite is a naturally occurring white mineral with an acicular (needle-shaped) particle structure. This distinctive particle morphology makes wollastonite an ideal performance mineral for a br.. |
|||
Bulk Density | 1.38 g/cc | 0.0499 lb/in³ | |
Inhance Fluoro-Seal INHANCE® Si-8220 Polymer Alloy Product Description: INHANCE S i-8000 series polymer alloy consists of black, medium density, silicon carbide chemically modified for greater adhesion. This product was designed for alloying with v.. |
|||
Bulk Density | 1.38 g/cc | 0.0499 lb/in³ | |
Inhance Fluoro-Seal INHANCE® Si-8900 Polymer Alloy Product Description: INHANCE S i-8000 series polymer alloy consists of black, medium density, silicon carbide chemically modified for greater adhesion. This product was designed for alloying with v.. |