Polymer Property : Bulk Density = 0.0394 lb/in³ Product List

Physical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Physical Properties Metric English Comments
Bulk Density 1.09 g/cc
0.0394 lb/in³
Loose
Excalibar ExBar™ W 3 Barite BaSO4 Powder
ExBar™ W high-purity white barytes are manufactured using only the highest quality white, natural barium sulfate ore. Strict quality control results in consistent products that are used in paints, ..
Bulk Density 1.09 g/cc
0.0394 lb/in³
Tapped
CIMBAR CIMTUFF® 9110 Talc
CIMTUFF® 9100 Series talcs are produced from high purity ore, which provides low iron content, low surface area and excellent color in dry form as well as when incorporated with resins. CIMTUFF® ..
Bulk Density 1.09 g/cc
0.0394 lb/in³
Tapped
CIMBAR MV 610 Talc
MV Series talcs are produced from high purity talc ore, which provide good color, acid resistance and excellent barrier properties when used in paint & coating formulations. MV Series talcs are pla..
Bulk Density 1.09 g/cc
0.0394 lb/in³
Tapped
CIMBAR RP 9405 Talc
RP 9400 Series talcs are produced from ores, which provide an excellent balance of mechanical properties at an economical price, for primary use in commodity polypropylene. RP 9400 Series talcs are..