Physical Properties | Metric | English | Comments |
---|---|---|---|
Bulk Density | 1.08 g/cc | 0.0390 lb/in³ | |
DuPont™ Nomex® 410 Paper, 25.5 mil Nominal Thickness Nomex® Type 410 is a calendared insulation paper which offers high inherent dielectric strength, mechanical toughness, flexibility, and resilience. It is the original form of Nomex® paper and is .. |