Physical Properties | Metric | English | Comments |
---|---|---|---|
Bulk Density | 1.05 g/cc | 0.0379 lb/in³ | |
Nabaltec NABALOX® NO 652 Reactive Alumina NABALOX® aluminum oxide has a number of advantages including low sintering temperaturewide sintering rangeflexible processinghigh sintered densities high wear and impact resistanceelectrical insula.. |
|||
Bulk Density | <= 1.05 g/cc | <= 0.0379 lb/in³ | |
Magyar Aluminum ALOLT 2AF Aluminum Hydroxide Ground type |
|||
Bulk Density | 1.05 - 1.15 g/cc | 0.0379 - 0.0415 lb/in³ | After drying at 110°C |
Gouda Vuurvast GOLITE 1.2.4. MIX GM Refractory Insulating Castable Description: This light weight gunning castable is composed of 1 part cement, 2 parts light weight grains and 4 parts vermiculite. Special additives provide for higher strength and less shrinkage.Re.. |
|||
Bulk Density | 1.05 - 1.15 g/cc | 0.0379 - 0.0415 lb/in³ | After drying at 110°C |
Gouda Vuurvast GOLITE LW Refractory Insulating Castable Description: This light weight (LW) castable can be used as a hot face material, as well as for the backlining of a dense castable or brickwork.Remarks: These values apply to cast products. Also ava.. |
|||
Bulk Density | 1.05 - 1.15 g/cc | 0.0379 - 0.0415 lb/in³ | After drying at 110°C |
Gouda Vuurvast GOLITE 120 Refractory Insulating Castable Description: Golite 120 is composed of light weight aggregates, alumina cement and special additions to be sure of a high strength and a low firing shrinkage.Remarks: These values apply to cast prod.. |
|||
Bulk Density | 1.05 g/cc | 0.0379 lb/in³ | Powder Density; ISO 60 |
Vyncolit X655 Novolac Phenolic Glass fiber and mineral filled phenolic molding compound with excellent dimensional stability and a very low coefficient of thermal expansion. UL listed.USES: Automotive disc brake pistons and gask.. |