Physical Properties | Metric | English | Comments |
---|---|---|---|
Bulk Density | 0.822 g/cc | 0.0297 lb/in³ | Poured; ASTM D1895 |
Eastman CA12 PET
(discontinued **) Voridian Polymer CA12 is currently produced to Voridian’s specifications and quality requirements by several resin manufacturers located in the Asis Pacific Region. Voridian Polymer CA12 offers imp.. |