Physical Properties | Metric | English | Comments |
---|---|---|---|
Bulk Density | 0.0220 - 0.0260 g/cc | 0.000795 - 0.000939 lb/in³ | |
BASF Neopolen® P 9225 K 0.04 g/cc Core density; Expanded Polypropylene (Europe) Description: Neopolen® P 9225 K is expanded Polypropylene supplied in the form of beads. The cells are largely closed.Physical properties of moldings made from Neopolen® P 9225 K.Note: In order to.. |
|||
Bulk Density | 0.0220 - 0.0260 g/cc | 0.000795 - 0.000939 lb/in³ | |
BASF Neopolen® P 9225 K 0.05 g/cc Core density; Expanded Polypropylene (Europe) Description: Neopolen® P 9225 K is expanded Polypropylene supplied in the form of beads. The cells are largely closed.Physical properties of moldings made from Neopolen® P 9225 K.Note: In order to.. |
|||
Bulk Density | 0.0220 - 0.0260 g/cc | 0.000795 - 0.000939 lb/in³ | |
BASF Neopolen® P 9225 K 0.06 g/cc Core density; Expanded Polypropylene (Europe) Description: Neopolen® P 9225 K is expanded Polypropylene supplied in the form of beads. The cells are largely closed.Physical properties of moldings made from Neopolen® P 9225 K.Note: In order to.. |
|||
Bulk Density | 0.0220 - 0.0260 g/cc | 0.000795 - 0.000939 lb/in³ | |
BASF Neopolen® P 9225 K 0.03 g/cc Core density; Expanded Polypropylene (Europe) Description: Neopolen® P 9225 K is expanded Polypropylene supplied in the form of beads. The cells are largely closed.Physical properties of moldings made from Neopolen® P 9225 K.Note: In order to.. |