Polymer Property : Bulk Density = 0.0191 lb/in³ Product List

Physical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Physical Properties Metric English Comments
Bulk Density 0.416 - 0.528 g/cc
0.0150 - 0.0191 lb/in³
Inhance Fluoro-Seal INHANCE® HD-1800 HDPE
Product Description: INHANCE HD-1000 Series Polyethylene Particles are surface-activated High Density Polyethylene (HDPE) in particle or powder form. Surface activation makes the particles easy to..
Bulk Density 0.416 - 0.528 g/cc
0.0150 - 0.0191 lb/in³
Inhance Fluoro-Seal INHANCE® HD-1035 HDPE
Product Description: INHANCE HD-1000 Series Polyethylene Particles are surface-activated High Density Polyethylene (HDPE) in particle or powder form. Surface activation makes the particles easy to..