Physical Properties | Metric | English | Comments |
---|---|---|---|
Bulk Density | 0.365 g/cc | 0.0132 lb/in³ | Pour Density; ASTM D 1513 |
Orion Engineered Carbons CORAX® N 550 ASTM Carbon Black Standard grade of furnace black in accordance with the requirements of ASTM D 1765Soft Black - carcass grade, semi-reinforcing carbon blackInformation provided by Orion Engineered Carbons. |
|||
Bulk Density | 0.365 g/cc | 0.0132 lb/in³ | Pour Density; ASTM D 1513 |
Orion Engineered Carbons PUREX® HS 45 Carbon Black Carbon black grade for manufacture of mechanical rubber goods such as extruded profiles and sealsInformation provided by Orion Engineered Carbons. |
|||
Bulk Density | 0.365 g/cc | 0.0132 lb/in³ | Pour Density; ASTM D 1513 |
Orion Engineered Carbons PUREX® HS 45-RP Carbon Black Carbon black grade for manufacture of mechanical rubber goods such as extruded profiles and sealsInformation provided by Orion Engineered Carbons. |