Physical Properties | Metric | English | Comments |
---|---|---|---|
Bulk Density | 0.00800 - 0.300 g/cc | 0.000289 - 0.0108 lb/in³ | |
BASF Neopolen® P 92HD 105 Expanded Polypropylene (Europe) Description: Neopolen® P 92HD 105 is expanded Polypropylene supplied in the form of beads. The cells are largely closedInformation provided by BASF |