Bulk Density 0.0390 - 0.0400 g/cc
0.00141 - 0.00145 lb/in³
BASF Styropor® P 340 EPS
Description: Expandable polystyrene (EPS) containing nominal 4.3 wt% pentane as the blowing agent.Intended uses: General purpose shape molding applications with fast molding cycles: Protective packa..
Bulk Density 0.0390 - 0.0400 g/cc
0.00141 - 0.00145 lb/in³
BASF Styropor® P 240 EPS
Description: Expandable polystyrene (EPS) containing nominal 4.3 wt% pentane as the blowing agent.Intended uses: Shape molding of thick walled parts, including: High density applications (greater th..
Bulk Density 0.0390 - 0.0400 g/cc
0.00141 - 0.00145 lb/in³
BASF Styropor® P 440 EPS
Description: Expandable polystyrene (EPS) containing nominal 4.3 wt% pentane as the blowing agent.Intended uses: Shape molding of thin walled parts with fast molding cycles including: Seedling trays..