Polymer Property : Spiral Flow = 6.30 in Product List

Physical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Physical Properties Metric English Comments
Spiral Flow 16.0 cm

@Thickness 1.00 mm
6.30 in

@Thickness 0.0394 in
395°C nozzle, 200°C tool
Victrex® ST™ STG45 PolyEtherKetoneEtherKetoneKetone, Unreinforced
Product Description:High performance thermoplastic material, unreinforced PolyEtherKetoneEtherKetoneKetone (PEKEKK), semi crystalline, depth filtered granules for injection moulding, standard flow, ..