Polymer Property : Spiral Flow = 300 cm Product List

Physical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Physical Properties Metric English Comments
Spiral Flow 300 cm

@Thickness 1.00 mm
118 in

@Thickness 0.0394 in
400°C nozzle, 200°C tool
Victrex® PEEK 150G / 151G Polyetheretherketone, Unreinforced
Product Description:High performance thermoplastic material, unreinforced Polyetheretherketone (PEEK), semi crystalline, depth filtered granules for injection moulding, easy flow, FDA food contact c..