Physical Properties | Metric | English | Comments |
---|---|---|---|
Spiral Flow | 53.0 cm @Temperature 260 °C |
20.9 in @Temperature 500 °F |
ASTM D3123 |
Total PS CPDS 850S Chlorine and Bromine Free Flame Retardant High Impact Polystyrene Total Petrochemicals Polystyrene 850S is a chlorine and bromine free flame retardant high impact polystyrene with excellent thermal stability and processability for injection molding.Suitable Applic.. |
|||
Spiral Flow | 53.0 cm @Temperature 260 °C |
20.9 in @Temperature 500 °F |
ASTM D3123 |
Total PS CPDS 855S Chlorine and Bromine Free Flame Retardant High Impact Polystyrene Total Petrochemicals Polystyrene 855S is a chlorine and bromine free flame retardant high impact polystyrene with excellent thermal stability and processability for injection molding.Suitable Applic.. |