Physical Properties | Metric | English | Comments |
---|---|---|---|
Spiral Flow | 10.0 cm @Thickness 1.00 mm |
3.94 in @Thickness 0.0394 in |
410°C nozzle, 210°C tool |
Victrex® ST™ ST45GL30 Polyetherketoneetherketoneketone (PEKEKK), 30% Glass Fiber Reinforced Product Description:High performance thermoplastic material, 30% glass fibre reinforced PolyEtherKetoneEtherKetoneKetone (PEKEKK), semi crystalline, granules for injection moulding, standard flow, c.. |