Physical Properties | Metric | English | Comments |
---|---|---|---|
Viscosity Measure | 80 cSt | 80 cSt | Toluene solution viscosity 5,23%; MA 04-3-003 |
Dynasol Calprene® H6170 Hydrogenated Rubber SEBS Calprene H 6170 is a 67/33 Ethylene-Butylene/Styrene thermoplastic copolymer, polymerized in solution and having a linear structure with excellent ozone resistance.This product is available in:CH 61.. |
|||
Viscosity Measure | 80 cSt | 80 cSt | 5.23% Toluene solution; MA-04-3-003 |
Dynasol Calprene® H6174 Hydrogenated Rubber (SEBS) Calprene H6174 is a 67/33 linear structure ethylene-butylene/styrene thermoplastic copolymer, polymerized in solution, with a high molecular weight and excellent ozone resistance. This product gives.. |