Physical Properties Metric English Comments
Viscosity Measure 250 - 600 cSt

@Temperature 20.0 °C
250 - 600 cSt

@Temperature 68.0 °F
Hong Kun Group AO 1135 Antioxidant
This product is phenols antioxidant, applicable to the occasion that there are liquor, latex, soliquoid and mixture,especially applicable to polyols and polyurethane.it has excellent effect in anti-..