Physical Properties | Metric | English | Comments |
---|---|---|---|
Viscosity Measure | 6.8 cSt | 6.8 cSt | Kinetic/Kinematic |
Dow Corning XIAMETER® PMCPPMX-0246 Cyclohexasiloxane Is chemically equivalent to DOW CORNING® 246 FLUID. This product is a volatile, low viscosity cyclohexasiloxane fluid for use in skincare, suncare, color cosmetics, hair care, and antiperspirant / .. |