Physical Properties Metric English Comments
Viscosity Measure 35 cSt
35 cSt
Styrene solution viscosity 5%; NM 300-11
Dynasol Calprene® 1015 Styrene-Butadiene Rubber SBR Diblock Copolymer
Calprene 1015 is a linear high molecular weight random-block styrene/butadiene copolymer with 15% styrene, 10% present as a polystyrene block. It has a non-staining antioxidant system; FDA approved ..
Viscosity Measure 35 cSt
35 cSt
Styrene solution viscosity 5%; NM 300-11
Dynasol Solprene® 1110 Styrene-Butadiene Rubber SBR Diblock Copolymer
Solprene 1110 is a linear high molecular weight random -block styrene-butadiene copolymer with 15% styrene, 10% present as a polystyrene block. It has a non staining antioxidant system, FDA approved..