Physical Properties | Metric | English | Comments |
---|---|---|---|
Viscosity Measure | 1800 - 3300 cSt | 1800 - 3300 cSt | Kinetic/Kinematic |
Dow Corning 3160 Antifoam Compound 100% active silicone fluid containing a suspension of finely powdered silica to enhance its defoaming efficiency.Information provided by Dow Corning |