Physical Properties | Metric | English | Comments |
---|---|---|---|
Viscosity Measure | 30000 cSt | 30000 cSt | Kinetic/Kinematic |
Dow Corning XIAMETER® PMCPPMX-200 30,000CS Silicone Fluid Is chemically equivalent to DOW CORNING® 200 FLUID 30,000CS. 100% active, 30,000 cSt, polydimethylsiloxane polymer.Information provided by Dow Corning |