Physical Properties Metric English Comments
Viscosity Measure 28 cSt
28 cSt
Toluene solution viscosity 5,23%; MA 04-3-003
Dynasol Calprene® 412 Thermoplastic Rubber SBS Dry
Calprene 412 is a 69/31 Butadiene/Styrene thermoplastic copolymer, polymerized in solution and has a radial structure.This product is available in:C 412 porous pelletC 412M powder form dusted with a..
Viscosity Measure 28 cSt
28 cSt
Toluene solution viscosity 5,23%; NM 300-11
Dynasol Solprene® 411 Thermoplastic Rubber SBS Dry
Solprene 411 is a 70/30 butadiene/styrene thermoplastic copolymer, polymerized in solution and has a radial structure.This product is available in:S 411 porous crumbS 411M powder form dusted with am..