Viscosity Measure 8.2 - 25 cSt
8.2 - 25 cSt
Average value: 17.4 cSt Grade Count:16
Overview of materials for Styrenic TPE  (Unverified Data**)
This property data is a summary of similar materials in the MatWeb database for the category "Styrenic TPE". Each property range of values reported is minimum and maximum values of appropriate MatWe..