Physical Properties Metric English Comments
Viscosity Measure 225 cSt
225 cSt
Kinetic/Kinematic
Dow Corning SYL-OFF® PMCP7671 Coating
Syl-Off® 7671 Coating is a 100% active solids, pre-catalysed, coating containing a low viscosity hexenyl endblocked only functional silicone polymer. Provides fast cure and stable premium release p..
Viscosity Measure 225 - 260 cSt

@Temperature 25.0 °C
225 - 260 cSt

@Temperature 77.0 °F
ASTM D445-94
Dow VORANOL™ CP 755 Polyol
VORANOL™ CP 755 polyol is a glycerine propoxylated polyether triol.Information provided by Dow