Physical Properties | Metric | English | Comments |
---|---|---|---|
Viscosity Measure | 18000 - 25000 cSt | 18000 - 25000 cSt | Kinetic/Kinematic |
Dow Corning 2-3898 Antifoam Compound 100% active silicone fluid containing a suspension of finely powdered silica to enhance its defoaming efficiency.Information provided by Dow Corning |